Rubber Shin-Etsu Elastomer KE-2090-50A/B Shin-Etsu Silicones of America
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer KE-2090-50A/B |
---|---|---|---|
Shore hardness | 50 |
thermosetting | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer KE-2090-50A/B |
---|---|---|---|
shelf-life | 32°C | 26 wk |
Uncured Properties | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer KE-2090-50A/B |
---|---|---|---|
Curing Time | 0.17 hr |
elastomer | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer KE-2090-50A/B |
---|---|---|---|
tear strength | 38.0 kN/m | ||
elongation | 断裂 | 420 % | |
compression set | 180°C,22hr | 9.0 % | |
tensile strength | 8.30 MPa |
physical property | Test Condition | Test Method | Shin-Etsu Silicones of America/Shin-Etsu Elastomer KE-2090-50A/B |
---|---|---|---|
density | 1.12 g/cm³ |