Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

K(Q)胶 KR-03NW CPCHEM KOREA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | CPCHEM KOREA/KR-03NW |
---|---|---|---|
Heat Deflection Temperature | 1.8MPa,未退火 | ASTMD648 | 62.2 °C |
Vicat Softening Temperature | ASTMD1525 | 85 °C |
Hardness | Test Condition | Test Method | CPCHEM KOREA/KR-03NW |
---|---|---|---|
Shore Hardness | 邵氏D | ASTMD2240 | 63 |
Physical | Test Condition | Test Method | CPCHEM KOREA/KR-03NW |
---|---|---|---|
Moisture Absorption | 24hr | ASTMD570 | 0.09 % |
Melt Mass-Flow Rate | 200°C/5.0kg | ASTMD1238 | 7.5 g/10min |
Mechanical Properties | Test Condition | Test Method | CPCHEM KOREA/KR-03NW |
---|---|---|---|
Flexural Modulus | 3.18mm | ASTMD790 | 1800 Mpa |
Tensile Elongation | 断裂 | ASTMD638 | 230 % |
Flexural Strength | 屈服,3.18mm | ASTMD790 | 37.2 Mpa |
Tensile Strength | 屈服 | ASTMD638 | 26.2 Mpa |
Optical | Test Condition | Test Method | CPCHEM KOREA/KR-03NW |
---|---|---|---|
60° | ASTMD2457 | 162 | |
Transmittance | ASTMD1003 | 92 % |
Impact Properties | Test Condition | Test Method | CPCHEM KOREA/KR-03NW |
---|---|---|---|
Instrumented Dart Impact | 23°C,3.18mm | ASTMD3763 | 40 J |
Flammability | Test Condition | Test Method | CPCHEM KOREA/KR-03NW |
---|---|---|---|
Flame Rating | UL94 | HB |