Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP Homopolymer Mineralblend® PP-2800 Colour Image Plastic Compound Sdn. Bhd. (CIPC)
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodColour Image Plastic Compound Sdn. Bhd. (CIPC)/Mineralblend® PP-2800
Impact strength of cantilever beam gap23°CASTM D25640 J/m
Mechanical propertiesTest ConditionTest MethodColour Image Plastic Compound Sdn. Bhd. (CIPC)/Mineralblend® PP-2800
elongation断裂ASTM D63810 %
tensile strength ASTM D63830.0 MPa
Flexural modulusASTM D7905400 MPa
bending strengthASTM D79052.0 MPa
flammabilityTest ConditionTest MethodColour Image Plastic Compound Sdn. Bhd. (CIPC)/Mineralblend® PP-2800
UL flame retardant rating1.6mmUL 94HB
physical property Test ConditionTest MethodColour Image Plastic Compound Sdn. Bhd. (CIPC)/Mineralblend® PP-2800
Shrinkage rateMD:3.20mmASTM D9550.60to1.0 %
melt mass-flow rate230°C/2.16kgASTM D12387.0 g/10min
densityASTM D7921.23 g/cm³
Thermal performanceTest ConditionTest MethodColour Image Plastic Compound Sdn. Bhd. (CIPC)/Mineralblend® PP-2800
Heat distortion temperature0.45MPa,未退火,4.00mm,HDTASTM D648140 °C
1.8MPa,未退火,4.00mm,HDTASTM D64890.0 °C