ETFE 207 CHEMOURS US
TEFZEL®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | CHEMOURS US/207 |
---|---|---|---|
Maximum operating temperature | UL 746 | 150 °C | |
Melting temperature | ASTM D3159 | 250to280 °C |
mechanical properties | Test Condition | Test Method | CHEMOURS US/207 |
---|---|---|---|
Bending modulus | 23°C | ASTM D790 | 1000 Mpa |
elongation | Break,23°C | ASTM D3159 | 300 % |
tensile strength | 23°C | ASTM D3159 | 40.0 Mpa |
Electrical performance | Test Condition | Test Method | CHEMOURS US/207 |
---|---|---|---|
Dielectric constant | 23°C,1MHz | ASTM D150 | 2.60to2.80 |
Dielectric strength | 0.250mm | ASTM D149 | 67 KV/mm |
Dissipation factor | 23°C,1MHz | ASTM D150 | 9E-03 |
Volume resistivity | ASTM D257 | 1E+17 ohms·cm |
Physical properties | Test Condition | Test Method | CHEMOURS US/207 |
---|---|---|---|
melt mass-flow rate | 297°C/5.0kg | ASTM D3159 | 30 g/10min |
Water absorption rate | 24hr | ASTM D570 | 7E-03 % |
flammability | Test Condition | Test Method | CHEMOURS US/207 |
---|---|---|---|
Extreme Oxygen Index | ASTM D2863 | 30to32 % |