| thermal performance | Test Condition | Test Method | HOTAI TAIWAN/795 |
|---|---|---|---|
| Brittle temperature | -50.0 °C | ||
| mechanical properties | Test Condition | Test Method | HOTAI TAIWAN/795 |
| Shore hardness | Shore D, 10 Sec | ASTM D2240 | 52 |
| Permanent compression deformation | 23℃, 70 hr | ASTM D395 | 24 % |
| elongation | Break | ASTM D412 | 540 % |
| Change rate of ultimate elongation in air | 125℃, 168 hr | ASTM D573 | -2.0 % |
| Change rate of tensile strength in air | 125℃, 168 hr | ASTM D573 | 1.0 % |
| Change rate of hardness (Shore) in the air | Shore A,125℃, 168 hr | ASTM D573 | 20 |
| tensile strength | 300%Strain | ASTM D412 | 6.28 Mpa |
| ASTM D412 | 8.83 Mpa | ||
| Physical properties | Test Condition | Test Method | HOTAI TAIWAN/795 |
| Shrinkage rate | MD | 0.50 % | |
| melt mass-flow rate | 190℃/2.16 kg | ASTM D1238 | 13 g/10 min |
| Shrinkage rate | TD | 0.90 % |