PPS A310MB7 TORAY PLASTICS CHENGDU
Torelina®
Fiber grade
Flame retardant、Glass fiber reinforced、Mineral reinforcement、High rigidity、high strength、High temperature resistan
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | TORAY PLASTICS CHENGDU/A310MB7 |
---|---|---|---|
Water absorption rate | ASTM D-570 | 0.02 % |
Electrical performance | Test Condition | Test Method | TORAY PLASTICS CHENGDU/A310MB7 |
---|---|---|---|
ASTM D-495 | 182 秒 | ||
Insulation breakdown voltage | ASTM D-149 | 15 MV/m | |
Induced positive connection | 10 | ASTM D-150 | 0.002 |
Inherent resistance of volume | ASTM D-257 | 10 Ω.m | |
permittivity | 10 | ASTM D-150 | 5.8 |
Mechanical properties | Test Condition | Test Method | TORAY PLASTICS CHENGDU/A310MB7 |
---|---|---|---|
Impact Strength | 缺口23℃ | ASTM D-256 | 90 J/m |
ASTM D-1044 | 70 mg/1000回 | ||
breaking strength | ASTM D-732 | 60 | |
tensile strength | ASTM D-638 | 1.2 % | |
bending strength | ASTM D-790 | 200 Mpa | |
Impact Strength | 无缺口23℃ | ASTM D-256 | 20 KJ/m |
hardness | ASTM D-785 | 123 洛氏 | |
Curved elastic body | ASTM D-790 | 17.6 GPa | |
Limit PV value | 东丽法 | 815 KJ/m | |
Tensile strength | ASTM D-638 | 140 Mpa | |
对钢 | ASTM D-1894 | 0.30 |
physical property | Test Condition | Test Method | TORAY PLASTICS CHENGDU/A310MB7 |
---|---|---|---|
Shrinkage rate | 流动方向 | 东丽法 | 0.15 % |
垂重方向 | 东丽法 | 0.55 % | |
320℃,98MPa,1mm厚 | 东丽法 | 90 |
Thermal performance | Test Condition | Test Method | TORAY PLASTICS CHENGDU/A310MB7 |
---|---|---|---|
1.82MPa | ASTM D-648 | >260 °C | |
DSC | 278 °C | ||
combustibility | UL-94 | V-0 | |
垂重方向 | ASTM D-696 | 2.4 | |
流动方向 | ASTM D-696 | 1.6 |