PP TechnoFin PP GF 20 TECHNOCOMPOUND GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodTECHNOCOMPOUND GERMANY/TechnoFin PP GF 20
Charpy Notched Impact Strength23°CISO 179/1eA5.0 kJ/m²
-30°CISO 179/1eA4.1 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU30 kJ/m²
-30°CISO 179/1eU25 kJ/m²
hardnessTest ConditionTest MethodTECHNOCOMPOUND GERMANY/TechnoFin PP GF 20
ball-indentation hardnessISO 2039-159.0 MPa
Electrical performanceTest ConditionTest MethodTECHNOCOMPOUND GERMANY/TechnoFin PP GF 20
Surface ResistivityIEC 600931E+13 ohms
Mechanical propertiesTest ConditionTest MethodTECHNOCOMPOUND GERMANY/TechnoFin PP GF 20
tensile strength 断裂ISO 527-2/555.0 MPa
Tensile strain断裂ISO 527-2/53.4 %
Flexural modulusISO 1784010 MPa
Tensile modulusISO 527-2/13500 MPa
Tensile strain屈服ISO 527-2/503.0 %
tensile strength 屈服ISO 527-2/5045.0 MPa
bending strengthISO 17884.9 MPa
physical property Test ConditionTest MethodTECHNOCOMPOUND GERMANY/TechnoFin PP GF 20
densityISO 11831.03 g/cm³
Melt volume flow rate230°C/2.16kgISO 113314.0 cm³/10min
Thermal performanceTest ConditionTest MethodTECHNOCOMPOUND GERMANY/TechnoFin PP GF 20
Heat distortion temperature0.45MPa,未退火,HDTISO 75-2/B155 °C
1.8MPa,未退火,HDTISO 75-2/A119 °C