Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM 150 NC010 DUPONT USA
Delrin®
household electrical appliances,Fitness equipment
UV resistance,wear resistant,High temperature resistan
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | DUPONT USA/150 NC010 |
|---|---|---|---|
| Emission | VDA275 | <8.00 mg/kg |
| hardness | Test Condition | Test Method | DUPONT USA/150 NC010 |
|---|---|---|---|
| Rockwell hardness | M-Sale | ISO 2039-2 | 94 |
| R-Sale | ISO 2039-2 | 122 |
| thermal performance | Test Condition | Test Method | DUPONT USA/150 NC010 |
|---|---|---|---|
| AnnealingTemperature | 160 °C | ||
| AnnealingTime-Optional | 30.0 min/mm | ||
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 165 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 97.0 °C | |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1E-04 cm/cm/°C |
| MD | ISO 11359-2 | 1.1E-04 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 178 °C |
| mechanical properties | Test Condition | Test Method | DUPONT USA/150 NC010 |
|---|---|---|---|
| Bending modulus | ISO 178 | 2900 Mpa | |
| Nominal tensile fracture strain | ISO 527-2 | 40 % | |
| Tensile modulus | ISO 527-2 | 3100 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 22 % |
| tensile strength | Yield | ISO 527-2 | 72.0 Mpa |
| Physical properties | Test Condition | Test Method | DUPONT USA/150 NC010 |
|---|---|---|---|
| melt mass-flow rate | ISO 1133 | 2.4 g/10min | |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 1.90 cm3/10min |
| Shrinkage rate | MD | ISO 294-4 | 1.8 % |
| TD | ISO 294-4 | 2.0 % |
| flammability | Test Condition | Test Method | DUPONT USA/150 NC010 |
|---|---|---|---|
| Burning rate | 1.00mm | ISO 3795 | <100 mm/min |
| Flammability level | 1.5mm | IEC 60695-11-10,-20 | HB |
| FMVSS flammability | FMVSS302 | B | |
| UL flame retardant rating | 1.5mm | UL 94 | HB |