Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPO AURAPENE PPTF30BK Aurora Manufacturing Ltd
--
currency
Filler, talc filler, 30%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Aurora Manufacturing Ltd/AURAPENE PPTF30BK |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/B | >5.2 kJ/m² | |
Impact strength of cantilever beam gap | ISO 180 | >3.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | Aurora Manufacturing Ltd/AURAPENE PPTF30BK |
---|---|---|---|
tensile strength | 屈服 | ISO 527-2 | 28.0 MPa |
Flexural modulus | ISO 178 | 3500 MPa |
flammability | Test Condition | Test Method | Aurora Manufacturing Ltd/AURAPENE PPTF30BK |
---|---|---|---|
burning rate | FMVSS302 | <100 mm/min | |
UL flame retardant rating | 内部方法 | HB |
physical property | Test Condition | Test Method | Aurora Manufacturing Ltd/AURAPENE PPTF30BK |
---|---|---|---|
Shrinkage rate | 0.50to1.5 % | ||
density | ISO 1183 | 1.22 g/cm³ | |
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 15to20 g/10min |
Thermal performance | Test Condition | Test Method | Aurora Manufacturing Ltd/AURAPENE PPTF30BK |
---|---|---|---|
vicat | ISO 306/B50 | >100 °C |