Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP Sumitomo PP AZ564G SumiDurez Singapore Pte Ltd
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodSumiDurez Singapore Pte Ltd/Sumitomo PP AZ564G
Impact strength of cantilever beam gap23°CASTM D2569.0 kJ/m²
-20°CASTM D2565.0 kJ/m²
hardnessTest ConditionTest MethodSumiDurez Singapore Pte Ltd/Sumitomo PP AZ564G
Rockwell hardnessASTM D78586
Mechanical propertiesTest ConditionTest MethodSumiDurez Singapore Pte Ltd/Sumitomo PP AZ564G
Flexural modulusASTM D7901280 MPa
tensile strength 断裂ASTM D63816.0 MPa
屈服ASTM D63824.0 MPa
flammabilityTest ConditionTest MethodSumiDurez Singapore Pte Ltd/Sumitomo PP AZ564G
UL flame retardant ratingUL 94HB
physical property Test ConditionTest MethodSumiDurez Singapore Pte Ltd/Sumitomo PP AZ564G
Shrinkage rateMD内部方法1.4 %
melt mass-flow rate230°C/2.16kgASTM D123839 g/10min
Shrinkage rateTD内部方法1.6 %
densityASTM D792A0.900 g/cm³
Thermal performanceTest ConditionTest MethodSumiDurez Singapore Pte Ltd/Sumitomo PP AZ564G
Heat distortion temperature0.45MPa,未退火,HDTASTM D648118 °C
vicatASTM D15252149 °C

Contact Us

Get App

Top