Thermal Properties | Test Condition | Test Method | MITSUI CHEM SINGAPORE/A4085S |
---|---|---|---|
Brittleness Temperature | ASTMD746 | <-70.0 °C | |
Vicat Softening Temperature | ASTMD1525 | 55.0 °C | |
Melting temperature | ASTMD2117 | 66.0 °C |
Hardness | Test Condition | Test Method | MITSUI CHEM SINGAPORE/A4085S |
---|---|---|---|
Shore Hardness | 邵氏A | ASTMD2240 | 86 |
Physical | Test Condition | Test Method | MITSUI CHEM SINGAPORE/A4085S |
---|---|---|---|
Melt Mass-Flow Rate | 190°C/2.16kg | ASTMD1238 | 3.6 g/10min |
230°C/2.16kg | ASTMD1238 | 6.7 g/10min | |
Mooney Viscosity | ML1+4 | JISK6395 | 16 MU |
Mechanical Properties | Test Condition | Test Method | MITSUI CHEM SINGAPORE/A4085S |
---|---|---|---|
Torsional Rigidity | ASTMD1043 | 9.00 Mpa | |
Tensile Elongation | 断裂 | ASTMD638 | >1000 % |
Tensile Strength | 断裂 | ASTMD638 | >22.0 Mpa |
Electrical Properties | Test Condition | Test Method | MITSUI CHEM SINGAPORE/A4085S |
---|---|---|---|
Dissipation Factor? | ASTMD150 | <5.0E-4 | |
Volume Resistivity | ASTMD257 | >1.0E+17 ohms·cm | |
Dielectric Constant | ASTMD150 | 2.20to2.40 |