Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
POM K300EW KOLON KOREA
KOCETAL® 
currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodKOLON KOREA/K300EW
Rockwell hardnessM级ASTM D78580
M级ISO 2039-293
Mechanical propertiesTest ConditionTest MethodKOLON KOREA/K300EW
Tensile strain断裂,23°CISO 527-250 %
bending strength23°CISO 17887.0 Mpa
tensile strength 屈服,23°CISO 527-265.0 Mpa
Flexural modulus23°CISO 1782750 Mpa
bending strength23°CASTM D79091.0 Mpa
tensile strength 屈服,23°CASTM D63862.0 Mpa
elongation屈服,23°CASTM D63870 %
Flexural modulus23°CASTM D7902500 Mpa
Electrical performanceTest ConditionTest MethodKOLON KOREA/K300EW
Volume resistivityASTM D2571E+14 ohms·cm
dielectric strengthIEC 60243-119 KV/mm
Surface ResistivityASTM D2571E+16 ohms
Volume resistivityIEC 600931E+14 ohms·cm
Dissipation Factor1MHzASTM D1506E-03
dielectric strengthASTM D14919 KV/mm
Surface ResistivityIEC 600931E+16 ohms
dielectric constantASTM D1503.70
flammabilityTest ConditionTest MethodKOLON KOREA/K300EW
UL flame retardant rating0.8mmUL 94HB
physical property Test ConditionTest MethodKOLON KOREA/K300EW
Shrinkage rateMDASTM D9552.0 %
TDISO 294-42.3 %
MDISO 294-42.4 %
Water absorption rate23°C,24hrISO 620.54 %
平衡,23°C,60%RHASTM D5700.22 %
melt mass-flow rate190°C/2.16kgASTM D12389.0 g/10min
190°C/2.16kgISO 11339.0 g/10min
Thermal performanceTest ConditionTest MethodKOLON KOREA/K300EW
Heat distortion temperature1.8MPa,未退火,HDTASTM D648110 °C
vicatASTM D1525162 °C
melting temperatureISO 11357-3166 °C
Heat distortion temperature0.45MPa,未退火,HDTASTM D648158 °C
1.8MPa,未退火,HDTISO 75-2/A95.0 °C
Linear coefficient of thermal expansionMDASTM D6961.3E-04 cm/cm/°C
melting temperature166 °C