Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

SEBS G7720-1001-01 KRATON USA
KRATON™
Household daily necessiti、sealant
Weather resistance、antioxidant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | KRATON USA/G7720-1001-01 |
---|---|---|---|
邵氏A | 内部方法 | 52到62 | |
邵氏A2 | 内部方法 | 62 | |
邵氏A,10秒 | 内部方法 | 57 |
Supplementary Information | Test Condition | Test Method | KRATON USA/G7720-1001-01 |
---|---|---|---|
OzoneResistance5 | 38°C | ASTMD518/1149 | NoCracking |
flammability | Test Condition | Test Method | KRATON USA/G7720-1001-01 |
---|---|---|---|
Burning rate 4 | FMVSS302 | 51 mm/min |
elastomer | Test Condition | Test Method | KRATON USA/G7720-1001-01 |
---|---|---|---|
Tensile stress flow rate | 300%应变,3.18mm | ASTMD412 | 2.07 Mpa |
500%应变 | ASTMD412 | 3.45 Mpa | |
Tensile strength flow rate | 屈服,3.18mm | ASTMD412 | 5.52 Mpa |
Tensile stress flow rate | 100%应变,3.18mm | ASTMD412 | 1.38 Mpa |
断裂,3.18mm | ASTMD412 | 700 % | |
Tear strength 3 | 3.18mm | ASTMD624 | 26.3 kN/m |
compression set | 23°C,22hr | ASTMD395B | 15 % |
70°C,22hr | ASTMD395B | 38 % |
aging | Test Condition | Test Method | KRATON USA/G7720-1001-01 |
---|---|---|---|
Change rate of tensile strength in air | 150°C,168hr | ASTMD573 | 140 % |
Change rate of ultimate elongation in air | ASTMD573 | 130 % | |
The rate of change in hardness of a hardness tester | 支撐A | ASTMD573 | 2.0 |
physical property | Test Condition | Test Method | KRATON USA/G7720-1001-01 |
---|---|---|---|
Shrinkage rate | MD | ASTMD955 | 1.4 % |
Thermal performance | Test Condition | Test Method | KRATON USA/G7720-1001-01 |
---|---|---|---|
brittle temperature | ASTMD746 | -63.0 °C |
Contact Us
Get App
Top