Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66/PTFE RBL-4036 SABIC INNOVATIVE US
LNP™ LUBRICOMP™
Lampholder cover,building materials,Gear cover
Low extract,Wear resistance,Corrosion resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/RBL-4036 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,64.0mmSpan7 | ISO 75-2/Af | 73.0 °C |
1.8MPa,Unannealed,3.20mm | ASTM D648 | 83.0 °C | |
0.45MPa,Unannealed,64.0mmSpan7 | ISO 75-2/Bf | 203 °C | |
0.45MPa,Unannealed,3.20mm | ASTM D648 | 236 °C | |
Linear coefficient of thermal expansion | TD:-30to30°C | ASTM D696 | 6.9E-05 cm/cm/°C |
MD:-30to30°C | ASTM D696 | 8.3E-05 cm/cm/°C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/RBL-4036 |
---|---|---|---|
Bending modulus | 50.0mmSpan4 | ASTM D790 | 3740 Mpa |
--5 | ISO 178 | 3570 Mpa | |
bending strength | ISO 178 | 107 Mpa | |
elongation | Break | ISO 527-2/5 | 8.3 % |
Yield3 | ASTM D638 | 8.5 % | |
Break3 | ASTM D638 | 10 % | |
Friction coefficient | Dynamic | ASTM D3702Modified | 0.47 |
Static | ASTM D3702Modified | 0.44 | |
Tensile modulus | --2 | ASTM D638 | 3990 Mpa |
-- | ISO 527-2/1 | 3930 Mpa | |
tensile strength | Break | ISO 527-2/5 | 64.0 Mpa |
Break3 | ASTM D638 | 64.0 Mpa | |
Wear factor | Ring | ASTM D3702Modified | 8.00 10^-10in^5-min/ft-lb-hr |
Washer | ASTM D3702Modified | 41.0 10^-10in^5-min/ft-lb-hr |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/RBL-4036 |
---|---|---|---|
Shrinkage rate | TD:24hr | ASTM D955 | 1.0-3.0 % |
MD:24hr | ASTM D955 | 2.0-4.0 % | |
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.58 % |
24hr,50%RH | ASTM D570 | 0.41 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/RBL-4036 |
---|---|---|---|
Dart impact | 23°C,TotalEnergy | ASTM D3763 | 5.60 J |
-- | ISO 6603-2 | 1.34 J | |
Suspended wall beam without notch impact strength | 23°C6 | ISO 180/1U | 27 kJ/m² |
23°C | ASTM D4812 | 440 J/m |