Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 B3 GF 15 1 L BK AKRO-PLASTIC GERMANY
AKROMID®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 15 1 L BK |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 60 kJ/m² |
-30°C | ISO 179/1eU | 60 kJ/m² |
Supplementary Information | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 15 1 L BK |
---|---|---|---|
ReinforcementContent | ISO 1172 | 15 % |
Mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 15 1 L BK |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 5200 Mpa | |
tensile strength | 断裂 | ISO 527-2/5 | 105 Mpa |
Tensile strain | 断裂 | ISO 527-2/5 | 3.3 % |
flammability | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 15 1 L BK |
---|---|---|---|
burning rate | 1.00mm | FMVSS302 | <100 mm/min |
Burning wire flammability index | 0.8mm | IEC 60695-2-12 | 700 °C |
UL flame retardant rating | 0.8mm | UL 94 | HB |
Hot filament ignition temperature | 0.8mm | IEC 60695-2-13 | 725 °C |
physical property | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 15 1 L BK |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 0.90 % |
MD | ISO 294-4 | 0.50 % | |
moisture absorption | 70°C,62%RH | ISO 1110 | 1.7 % |
spiral flow length | 内部方法 | 100 CM | |
Melt volume flow rate | 275°C/5.0kg | ISO 1133 | 15.0 cm3/10min |
Thermal performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/B3 GF 15 1 L BK |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 215 °C |
melting temperature | DIN EN11357-1 | 220 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 192 °C |