plas

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA6 B3EG3 BASF GERMANY
Ultramid® 
Automotive sector,wheel,Shell,Application in the automotive field,wheel,Shell
Oil resistant,High impact resistance,Filler: Glass fiber reinf,15% filler by weight
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodBASF GERMANY/B3EG3
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B217 °C
1.8MPa,UnannealedISO 75-2/A200 °C
Melting temperatureISO 3146220 °C
mechanical propertiesTest ConditionTest MethodBASF GERMANY/B3EG3
Bending modulus23°CISO 1785300 Mpa
Tensile modulus23°CISO 527-26060 Mpa
Tensile strainBreak,23°CISO 527-22.5 %
tensile strengthBreak,23°CISO 527-2115 Mpa
Electrical performanceTest ConditionTest MethodBASF GERMANY/B3EG3
Dielectric constant1MHzIEC 602503.80
Dissipation factor1MHzIEC 602500.025
100HzIEC 602500.025
Volume resistivityIEC 600931E+13 ohms·cm
Physical propertiesTest ConditionTest MethodBASF GERMANY/B3EG3
densityISO 11831.23 g/cm³
Water absorption rateEquilibrium,23°C,50%RHISO 622.3 %
Saturation,23°CISO 627.7 %
impact performanceTest ConditionTest MethodBASF GERMANY/B3EG3
Charpy Notched Impact Strength23°CISO 1795.0 kJ/m²
Impact strength of cantilever beam gap23°CISO 1805.0 kJ/m²
-30°CISO 1804.5 kJ/m²