Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPA AS-1133 BK324 SOLVAY USA
AMODEL®
Automotive components、Laptop case、Fitness equipment、Food contact parts、Plumbing components、Valves/valve components、Industrial applications、Industrial components、Metal substitution、Lawn and garden equipment、Power/Other Tools、Oil/Gas Supplies、currency、Parts under the hood of a、Application in the automo、Fuel pipeline、Machine/mechanical compon、Vehicle electronics、Shell、Thick wall accessories (c
enhance、Thermal stability、Dimensional stability、High temperature resistan、Filler: Glass fiber reinf、33% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Linear thermal expansion coefficient | TD:0to100°C | ASTME831 | 5.9E-05 cm/cm/°C |
Heat Deflection Temperature | 1.8MPa,退火,3.18mm | ASTMD648 | 285 °C |
1.8MPa,退火 | ISO75-2/Af | 277 °C | |
Continuous Use Temperature | --3 | ASTMD3045 | 185 °C |
Linear thermal expansion coefficient | MD:160to249°C | ASTME831 | 1.4E-05 cm/cm/°C |
Continuous Use Temperature | --2 | ASTMD3045 | 164 °C |
Melting temperature | ISO11357-3 | 310 °C | |
Linear thermal expansion coefficient | MD:0to100°C | ASTME831 | 2.3E-05 cm/cm/°C |
TD:160to249°C | ASTME831 | 1.3E-04 cm/cm/°C | |
Heat Deflection Temperature | 0.45MPa,退火,3.18mm | ASTMD648 | 297 °C |
Peak Melting Temperature | ASTMD3418 | 310 °C |
Hardness | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Rockwell Hardness | R级 | ASTMD785 | 125 |
Mechanical Properties | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Tensile Elongation | 断裂 | ASTMD638 | 2.5 % |
Flexural Modulus | ASTMD790 | 10300 Mpa | |
Tensile Stress | 屈服 | ISO527-2 | 225 Mpa |
Poisson Ratio | 7.58 | 0.41 | |
Flexural Modulus | ISO178 | 10300 Mpa | |
Flexural Strength | 屈服 | ASTMD790 | 317 Mpa |
Tensile Strain | 断裂 | ISO527-2 | 3.0 % |
Compressive Strength | ASTMD695 | 276 Mpa | |
Flexural Stress | ISO178 | 326 Mpa | |
Tensile Modulus | ASTMD638 | 13100 Mpa | |
ISO527-2 | 12200 Mpa | ||
Shearing Strength | ASTMD732 | 101 Mpa | |
Tensile Strength | 断裂 | ASTMD638 | 221 Mpa |
Physical | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Moisture Absorption | 24hr | ASTMD570 | 0.21 % |
Modeling Shrinkage | TD | ASTMD955 | 0.80 % |
MD | ASTMD955 | 0.40 % |
Optical | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Light Transmittance | 940nm:1.60mm | ASTMD1003 | >30 % |
1070nm:1.60mm | ASTMD1003 | >35 % |
Impact Properties | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Charpy Unnotched Impact Strength | ISO179/1eU | 82 kJ/m² |
Flammability | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Flame Rating | 3.2mm | UL94 | HB |
Electrical Properties | Test Condition | Test Method | SOLVAY USA/AS-1133 BK324 |
---|---|---|---|
Comparative Tracking Index | CTI | UL746 | 550 V |
Volume Resistivity | ASTMD257 | 1E+16 ohms·cm | |
Dissipation Factor? | 60Hz | ASTMD150 | 5E-03 |
1MHz | ASTMD150 | 0.017 | |
Dielectric Constant | 60Hz | ASTMD150 | 4.40 |
Arc Resistance | ASTMD495 | 140 sec | |
Dielectric Constant | 1MHz | ASTMD150 | 4.20 |
Dielectric Strength | 3.17mm | ASTMD149 | 21 KV/mm |