| mechanical properties | Test Condition | Test Method | BOREALIS EUROPE/ED086T |
|---|---|---|---|
| Impact strength of cantilever beam gap | -40℃ | ISO 180/1A | 9.5 KJ/m |
| Tensile strain | Injection成型,Break | ISO 527-2/100 | 560 % |
| Shore hardness | ShoreD,Injection成型 | ISO 868 | 62 |
| Physical properties | Test Condition | Test Method | BOREALIS EUROPE/ED086T |
| Shrinkage rate | ISO 294-4 | 1.4 % | |
| thermal performance | Test Condition | Test Method | BOREALIS EUROPE/ED086T |
| Vicat softening temperature | ISO 306/A50 | 119 ℃ | |
| Basic Performance | Test Condition | Test Method | BOREALIS EUROPE/ED086T |
| melt mass-flow rate | 230°C/5.0 kg | ISO 1133 | 23 g/10 min |