Impact resistance | Test Condition | Test Method | EMS-GRIVORY/Grilamid® TR XE 4139 black 9231 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | kJ/m² | 11 12 |
-30°C | kJ/m² | 11 12 | |
Impact strength of simply supported beam without notch | 23°C | 无断裂 | |
-30°C | 无断裂 |
hardness | Test Condition | Test Method | EMS-GRIVORY/Grilamid® TR XE 4139 black 9231 |
---|---|---|---|
ball-indentation hardness | MPa | 160 160 |
Mechanical properties | Test Condition | Test Method | EMS-GRIVORY/Grilamid® TR XE 4139 black 9231 |
---|---|---|---|
Tensile modulus | MPa | 2800 2800 | |
tensile strength | 屈服 | MPa | 105 95.0 |
Tensile strain | 断裂 | % | 25 >50 |
屈服 | % | 7.0 6.0 |
Electrical performance | Test Condition | Test Method | EMS-GRIVORY/Grilamid® TR XE 4139 black 9231 |
---|---|---|---|
Surface Resistivity | ohms | -- 1E+12 | |
Compared to the Leakage Tracking Index (CTI) | V | -- | |
Volume resistivity | ohms·cm | 1E+13 1E+13 | |
dielectric strength | kV/mm | 27 27 |
flammability | Test Condition | Test Method | EMS-GRIVORY/Grilamid® TR XE 4139 black 9231 |
---|---|---|---|
Flammability level | 0.8mm | V-2 -- |
physical property | Test Condition | Test Method | EMS-GRIVORY/Grilamid® TR XE 4139 black 9231 |
---|---|---|---|
Shrinkage rate | MD | % | 0.70 -- |
density | g/cm³ | 1.15 -- | |
Water absorption rate | 饱和,23°C | % | 9.0 -- |
Shrinkage rate | TD | % | 0.70 -- |
Water absorption rate | 平衡,23°C,50%RH | % | 3.5 -- |
Thermal performance | Test Condition | Test Method | EMS-GRIVORY/Grilamid® TR XE 4139 black 9231 |
---|---|---|---|
Continuous use temperature | --2 | °C | 80.0to100 -- |
Heat distortion temperature | 0.45MPa,未退火,HDT | °C | 135 -- |
Continuous use temperature | --3 | °C | 120 -- |
Linear coefficient of thermal expansion | MD | cm/cm/°C | 6E-05 -- |
Heat distortion temperature | 1.8MPa,未退火,HDT | °C | 125 -- |
Glass Transition Temperature | °C | 160 -- | |
Linear coefficient of thermal expansion | TD | cm/cm/°C | 6E-05 -- |