Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC/PET X8303CL NA9A002T SABIC INNOVATIVE NANSHA
XYLEX™
household electrical appliances,Office supplies,label
UV resistance,High mobility,High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/X8303CL NA9A002T |
---|---|---|---|
0.45MPa, unannealed, 3.20mm | ASTM D648 | 92.0 °C | |
1.8MPa, unannealed, 3.20mm | ASTM D648 | 80.0 °C | |
1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 90.0 °C | |
Flow: 23 to 60 ° C | 23to60℃ | ISO 11359-2 | 9.2E-05 cm/cm/°C |
Flow: -40 to 40 ° C | ASTME831 | 9E-05 cm/cm/°C | |
Horizontal: 23 to 60 ° C | Across Flow, 23to60℃ | ISO 11359-2 | 9.8E-05 cm/cm/°C |
Horizontal: -40 to 40 ° C | Across Flow, -40to40℃ | ASTME831 | 9E-05 cm/cm/°C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/X8303CL NA9A002T |
---|---|---|---|
--1 | ASTM D638 | 1680 Mpa | |
50.0mm span | ASTM D790 | 1620 Mpa | |
--7 | ISO 178 | 1720 Mpa | |
--8 | ISO 178 | 72.0 Mpa | |
crack | ISO 527-2/50 | 140 % | |
ASTM D638 | 44.0 Mpa | ||
ASTM D638 | 140 % | ||
ISO 527-2/50 | 43.0 Mpa | ||
yield | ASTM D638 | 5.0 % | |
ASTM D638 | 46.0 Mpa | ||
ISO 527-2/50 | 6.0 % | ||
ISO 527-2/50 | 48.0 Mpa | ||
Yield, 50.0mm span | ASTM D790 | 72.0 Mpa |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/X8303CL NA9A002T |
---|---|---|---|
melt mass-flow rate | 265°C/2.16kg | ASTM D1238 | 30 g/10min |
Melt Volume Flow Rate (MVR) | 265°C/2.16kg | ISO 1133 | 27.5 cm3/10min |
Shrinkage rate | MD:3.20mm | Internal Method | 0.40-0.80 % |
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20 % |
Saturation,23°C | ISO 62 | 0.50 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE NANSHA/X8303CL NA9A002T |
---|---|---|---|
23°C | ASTM D256 | 1000 J/m | |
ISO 180/1A | 20 kJ/m² | ||
-30°C | ASTM D256 | 100 J/m | |
ISO 180/1A | 9.0 kJ/m² | ||
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 14 kJ/m² |
Dart impact | 23°C,TotalEnergy | ASTM D3763 | 65.0 J |