| mechanical properties | Test Condition | Test Method | LUBRIZOL KOREA/S198A-5 KR |
|---|---|---|---|
| elongation | Break | 520 % | |
| tear strength | ASTM D-624 | 177 kN/m | |
| tensile strength | Yield | 49 MPa | |
| 100%Strain | ASTM D-412 | 15.7 Mpa | |
| Wear amount | ISO 4649 | 25 mm³ | |
| Permanent compression deformation | 23℃,22.0hr | ASTM D-395 | 20 % |
| tensile strength | 300%Strain | ≤2 | MPa |
| Physical properties | Test Condition | Test Method | LUBRIZOL KOREA/S198A-5 KR |
| Shrinkage rate | MD | ASTM D-955 | 0.80 % |
| Shore hardness | ShoreA | ASTM D-2240 | 98 |
| thermal performance | Test Condition | Test Method | LUBRIZOL KOREA/S198A-5 KR |
| Vicat softening temperature | ASTM D-1525 | 143 °C |