Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC TR1501A SUMITOMO JAPAN
SD POLYCA™
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | SUMITOMO JAPAN/TR1501A |
|---|---|---|---|
| Hot deformation temperature | 1.8 MPa1.80MPa | ISO 75/Af | 116 °C |
| Linear coefficient of thermal expansion | MDMD | ISO 11359-2 | 0.000070 cm/cm/℃ |
| TDTD | ISO 11359-2 | 0.000070 cm/cm/℃ |
| mechanical properties | Test Condition | Test Method | SUMITOMO JAPAN/TR1501A |
|---|---|---|---|
| Bending modulus | ISO 178 | 2300 Mpa | |
| bending strength | ISO 178 | 80 Mpa | |
| Tensile modulus | ISO 527-2 | 2300 Mpa | |
| Tensile strain | BreakBreak | ISO 527-2 | 30 % |
| Tensile stress | Yield | ISO 527-2 | 60 Mpa |
| flame retardant performance | Test Condition | Test Method | SUMITOMO JAPAN/TR1501A |
|---|---|---|---|
| UL flame retardant rating | 3.00 mm | UL 94 | V-2 |
| 0.35 mm | UL 94 | V-2 |
| Physical properties | Test Condition | Test Method | SUMITOMO JAPAN/TR1501A |
|---|---|---|---|
| density | ISO 1183 | 1.2 g/cm³ | |
| melt mass-flow rate | 300℃,1.20kg300℃,1.2kg | ISO 1133 | 150 g/10min |
| Melt Volume Flow Rate (MVR) | 300℃,1.2 kg300℃,1.2kg | ISO 1133 | 143 cm3/10min |
| Shrinkage rate | TDTD | Internal Method | 0.5-0.7 % |
| MDMD | Internal Method | 0.5-0.7 % | |
| Water absorption rate | 23℃,24hr23℃,24hrs | ISO 62 | 0.2 % |
| impact performance | Test Condition | Test Method | SUMITOMO JAPAN/TR1501A |
|---|---|---|---|
| Charpy Notched Impact Strength | UnnotchedUnnotched,23℃,5mm | ISO 179-1 | NB kJ/m² |
| NotchedNotched,23℃,4mm | ISO 179-1 | 6 kJ/m² |
| optical performance | Test Condition | Test Method | SUMITOMO JAPAN/TR1501A |
|---|---|---|---|
| Refractive index | ISO 489 | 1.582 | |
| Total Light Transmittance | 2mm2mm | ISO 13468 | 90 % |
| turbidity | 2 mm2mm | ISO 14782 | 0.3 % |