Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP EE109AE BOREALIS EUROPE
Daplen™
Automotive External Parts,Car bumper,Automotive External Parts
Easy to process,High impact resistance,High rigidity,filler,Mineral filler,20%,Filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | BOREALIS EUROPE/EE109AE |
---|---|---|---|
Ball Pressure Test | H132/10 | ISO 2039-1 | 26.0 Mpa |
thermal performance | Test Condition | Test Method | BOREALIS EUROPE/EE109AE |
---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 92.0 °C |
1.8MPa,Unannealed | ISO 75-2/A | 50.0 °C | |
Linear coefficient of thermal expansion | MD:-30to80°C | Internal Method | 5E-05 cm/cm/°C |
Vicat softening temperature | -- | ISO 306/B50 | 38.0 °C |
-- | ISO 306/A50 | 121 °C |
mechanical properties | Test Condition | Test Method | BOREALIS EUROPE/EE109AE |
---|---|---|---|
Bending modulus | ISO 178 | 1500 Mpa | |
bending strength | ISO 178 | 21.0 Mpa | |
Tensile modulus | ISO 527-2/1 | 1400 Mpa | |
Tensile strain | Break | ISO 527-2/50 | >300 % |
Yield | ISO 527-2/50 | 7.0 % | |
tensile strength | Yield | ISO 527-2/50 | 16.0 Mpa |
Physical properties | Test Condition | Test Method | BOREALIS EUROPE/EE109AE |
---|---|---|---|
density | ISO 1183 | 1.04 g/cm³ | |
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 13 g/10min |
Shrinkage rate | --2 | Internal Method | 0.65 % |
90°C,2hr | Internal Method | 0.10 % |
impact performance | Test Condition | Test Method | BOREALIS EUROPE/EE109AE |
---|---|---|---|
Charpy Notched Impact Strength | -20°C | ISO 179/1eA | 5.0 kJ/m² |
23°C | ISO 179/1eA | 40 kJ/m² | |
-30°C | ISO 179/1eA | 4.2 kJ/m² | |
Impact strength of cantilever beam gap | -20°C | ISO 180/1A | 6.1 kJ/m² |
23°C | ISO 180/1A | 41 kJ/m² | |
Impact strength of simply supported beam without notch | -20°C | ISO 179/1eU | 无断裂 |
23°C | ISO 179/1eU | 无断裂 |