Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | APPC SAUDI/1101R |
|---|---|---|---|
| Tensile modulus | 1mm/min | ISO 527-2 | 1500 Mpa |
| Elongation at Break | 50mm/min | ISO 527-2 | >50 % |
| Ball Pressure Test | H358/30 | ISO 2039-1 | 78 Mpa |
| tensile strength | 50mm/min | ISO 527-2 | 34 Mpa |
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eU | 2.5 kJ/m² |
| elongation at yield | 50mm/min | ISO 527-2 | 8 % |
| Impact strength of simply supported beam without notch | 23℃ | ISO 179/1eU | 110 kJ/m² |
| thermal performance | Test Condition | Test Method | APPC SAUDI/1101R |
| Hot deformation temperature | 0.45MPa | ISO 75-2 | 85 °C |
| Melting temperature | ISO 3146 | 163 °C | |
| Vicat softening temperature | A50(10N) | ISO 306 | 154 °C |
| Physical properties | Test Condition | Test Method | APPC SAUDI/1101R |
| melt mass-flow rate | 230℃,2.16kg | ISO 1133 | 24 g/10min |
| density | ISO 1183 | 0.91 g/cm³ |