Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC DX13354 SABIC INNOVATIVE US
LNP™ THERMOCOMP™
Automotive components、Electronic and electrical
Thermal stability、High mobility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DX13354 |
---|---|---|---|
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 124 °C | |
0.45MPa, Unannealed,3.20mm Span | ISO75-2/Bf | 127 °C | |
1.8MPa, Unannealed,3.20mm | ASTMD648 | 122 °C | |
Flow:-40 to 40°C | ISO11359-2 | 7.1E-05 cm/cm/°C | |
0.45MPa, Unannealed,3.20mm | ASTMD648 | 126 °C | |
Flow:-40 to 40°C | ASTME831 | 6.9E-05 cm/cm/°C | |
ASTME831,ISO11359-2 | 2.1E-05 cm/cm/°C |
Physical | Test Condition | Test Method | SABIC INNOVATIVE US/DX13354 |
---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.050到0.10 % |
Melt Mass-Flow Rate | 280°C/2.16kg | ASTMD1238 | 10 g/10min |
300°C/1.2kg | ASTMD1238 | 16 g/10min | |
Modeling Shrinkage | TD:3.20mm | 内部方法 | 0.20到0.40 % |
Melt Volume flow Rate | 300°C/1.2kg | ASTMD1238 | 13.0 cm3/10min |
Melt Mass-Flow Rate | 280°C/5.0kg | ASTMD1238 | 27 g/10min |
Mechanical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DX13354 |
---|---|---|---|
ASTMD638 | 8760 Mpa | ||
Break | ASTMD638 | 120 Mpa | |
fracture | ISO527-2/50 | 2.4 % | |
Break | ASTMD638 | 2.4 % | |
fracture | ISO527-2/50 | 120 Mpa |
Impact Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DX13354 |
---|---|---|---|
Charpy Unnotched Impact Strength | 23°C | ISO179/2U | 50 kJ/m² |
ASTMD256 | 150 J/m | ||
ASTMD4812 | 700 J/m | ||
ISO180/1A | 14 kJ/m² | ||
ISO180/1U | 40 kJ/m² |
Electrical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DX13354 |
---|---|---|---|
Dissipation Factor? | 5.00GHz | 内部方法 | 0.012 |
1.90GHz | 内部方法 | 0.013 | |
Dielectric Constant | 1.90GHz | 内部方法 | 3.44 |
5.00GHz | 内部方法 | 3.51 | |
1.10GHz | 内部方法 | 3.52 | |
Dissipation Factor? | 1.10GHz | 内部方法 | 0.014 |