Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PVC Sekisui PVC HA-24F Sekisui (Hong Kong) Limited
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | Sekisui (Hong Kong) Limited/Sekisui PVC HA-24F |
|---|---|---|---|
| temperature | 弯曲 (Flex) | JISK6745 | 86 °C |
| thermal performance | Test Condition | Test Method | Sekisui (Hong Kong) Limited/Sekisui PVC HA-24F |
|---|---|---|---|
| Heat loss | JISK6720-2 | <0.3 wt% | |
| Hot deformation temperature | 0.45MPa,Unannealed | JISK7207 | 95.0 °C |
| 1.8MPa,Unannealed | JISK7191-1 | 85.0 °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 7.0E-5到7.5E-5 cm/cm/°C |
| Vicat softening temperature | JISK7206 | 103 °C |
| mechanical properties | Test Condition | Test Method | Sekisui (Hong Kong) Limited/Sekisui PVC HA-24F |
|---|---|---|---|
| Bending modulus | JISK7171 | 2750 MPa | |
| bending strength | JISK7171 | 86.0 MPa | |
| Tensile strain | Break | JISK7113 | 80 % |
| tensile strength | Yield | JISK7113 | 58.0 MPa |
| Electrical performance | Test Condition | Test Method | Sekisui (Hong Kong) Limited/Sekisui PVC HA-24F |
|---|---|---|---|
| Dielectric constant | 60Hz | 3.08 | |
| 1MHz | 3.20to3.60 | ||
| Dielectric strength | 47to63 kV/mm | ||
| Volume resistivity | 23°C | 1E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | Sekisui (Hong Kong) Limited/Sekisui PVC HA-24F |
|---|---|---|---|
| Apparent density | JISK6720-2 | 0.50to0.60 g/cm³ | |
| Chlorine content | ISO 1158 | 64.0 wt% | |
| density | JISK7112 | 1.53 g/cm³ | |
| K-Value | JISK6720-2 | 58.0 |
| impact performance | Test Condition | Test Method | Sekisui (Hong Kong) Limited/Sekisui PVC HA-24F |
|---|---|---|---|
| Impact strength of simply supported beam without notch | JISK7111 | 25 kJ/m² |