POE 8003 DOW THAILAND
ENGAGE™
Food packaging
Weather resistance、High temperature resistan、Toughening
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
film | Test Condition | Test Method | DOW THAILAND/8003 |
---|---|---|---|
Shrinking and stretching | MD:135°C | 内部方法 | 1.21 Mpa |
tensile strength | TD:屈服 | ASTMD882 | 55.8 Mpa |
elongation | MD:断裂 | ASTMD882 | 70 % |
Elmondov tear strength TD | 25µm | ASTMD1922 | 7.0 g |
Available film thickness | 1.0;1.15;1.25;1.5;2.0;2.5;3.0mil(25;29;32;38;51;64;76µ | ||
elongation | TD:断裂 | ASTMD882 | 90 % |
Shrinking and stretching | TD:135°C | 内部方法 | 0.896 Mpa |
Secant modulus | 1%正割,MD | ASTMD882 | 2480 Mpa |
usage | 38.1µm | ASTMD4321 | 25.0 m²/kg |
76.2µm | ASTMD4321 | 12.6 m²/kg | |
25.4µm | ASTMD4321 | 38.0 m²/kg | |
50.8µm | ASTMD4321 | 18.9 m²/kg | |
63.5µm | ASTMD4321 | 15.2 m²/kg | |
Secant modulus | 1%正割,TD | ASTMD882 | 2550 Mpa |
usage | 31.8µm | ASTMD4321 | 30.0 m²/kg |
Falling hammer impact | ASTMD1709 | 200 g | |
usage | 29.2µm | ASTMD4321 | 33.0 m²/kg |
tensile strength | MD:屈服 | ASTMD882 | 55.8 Mpa |
optical performance | Test Condition | Test Method | DOW THAILAND/8003 |
---|---|---|---|
gloss | 60° | ASTMD2457 | 20 |
Haze ratio | ASTMD1003 | 56 % |