Mechanical properties | Test Condition | Test Method | 土耳其EPSAN/EPLAMID 66 GFS 25 HS NC |
---|---|---|---|
Impact strength of cantilever beam gap | 23℃ | ISO 180/1A | 9 KJ/m² |
tensile strength | 23℃,断裂 | ISO 527-2 | 145 N/mm² |
bending strength | 23℃ | ISO 178 | 205 N/mm² |
hardness | ISO 868 | 88 | |
Tensile modulus | 23℃ | ISO 527-2 | 7500 N/mm² |
Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 10 KJ/m² |
Tensile stress | 23℃,断裂 | ISO 527-2 | 2 % |
Flexural modulus | 23℃ | ISO 178 | 7200 N/mm² |
other | Test Condition | Test Method | 土耳其EPSAN/EPLAMID 66 GFS 25 HS NC |
---|---|---|---|
UL flame retardant rating | UL -94 | HB |
physical property | Test Condition | Test Method | 土耳其EPSAN/EPLAMID 66 GFS 25 HS NC |
---|---|---|---|
water content | ISO 15512 | 0.2 % | |
Shrinkage rate | ISO 294-4 | 0.3-0.6 % | |
density | 23℃ | ISO 1183 | 1.28 g/cm³ |
ash content | ISO 3451-4 | 25 % |
Thermal performance | Test Condition | Test Method | 土耳其EPSAN/EPLAMID 66 GFS 25 HS NC |
---|---|---|---|
Hot deformation temperature (HDT) | HDT | ISO 75-2/A | 250 ℃ |
melting temperature | ISO 3146 | 250 ℃ | |
vicat | ISO 306/B50 | 255 ℃ | |
Hot deformation temperature (HDT) | HDT | ISO 75-2/B | 255 ℃ |