Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Jampilen H2150 Jam Polypropylene Company
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2150 |
---|---|---|---|
Impact strength of cantilever beam gap | 0°C | ISO 180/A | 2.5 kJ/m² |
23°C | ISO 180/A | 6.0 kJ/m² | |
-30°C | ISO 180/A | 1.5 kJ/m² |
hardness | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2150 |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 70 |
Mechanical properties | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2150 |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 1400 MPa | |
Tensile strain | 屈服 | ISO 527-2/50 | 9.0 % |
tensile strength | 屈服 | ISO 527-2/50 | 31.0 MPa |
physical property | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2150 |
---|---|---|---|
density | ISO 1183 | 0.900 g/cm³ | |
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 0.30 g/10min |
Thermal performance | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2150 |
---|---|---|---|
vicat | ISO 306/A50 | 150 °C | |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 90.0 °C |
melting temperature | ISO 3146 | 165 °C |