ABS 0646 NIZHNEKAMSKNEFTEKHIM RUSSIA
--
Wear resistant accessorie、Profile
heat-resisting、High impact resistance、High mobility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | DIN53453 | 12 kJ/m² |
23°C | ISO180 | 12 kJ/m² |
hardness | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
Rockwell hardness | R计秤 | ISO2039-2 | 110 |
Supplementary Information | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
ResidualStyrene3 | 内部方法 | 0.050 % |
Mechanical properties | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
elongation | 断裂 | ASTMD638 | 45 % |
Flexural modulus | ASTMD790 | 2300 Mpa | |
tensile strength | 屈服 | ASTMD638 | 43.0 Mpa |
bending strength | 屈服 | ASTMD790 | 65.0 Mpa |
optical performance | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
Gardner glossiness | 60° | ASTMD523 | 60 |
flammability | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
Hot filament ignition temperature | IEC60695-2-1 | 650 °C | |
UL flame retardant rating | UL94 | HB |
physical property | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
Shrinkage rate | MD | 0.40到0.60 % | |
melt mass-flow rate | 220°C/10.0kg | ASTMD1238 | 4.5到7.5 g/10min |
Water absorption rate | 平衡 | ASTMD570 | 0.30 % |
Thermal performance | Test Condition | Test Method | NIZHNEKAMSKNEFTEKHIM RUSSIA/0646 |
---|---|---|---|
MD | ASTMD696 | 9E-05 cm/cm/°C | |
thermal conductivity | ASTMC177 | 0.17 W/m/K | |
ASTMD15252 | 104 °C | ||
Heat distortion temperature | ASTMD648 | 108 °C |