Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
ABS XR-401 CNOOC&LG HUIZHOU
--
Electronic field,Electrical field
heat-resisting
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodCNOOC&LG HUIZHOU/XR-401
burning rate1/8"IEC 707FH3-33 mm/min
1/16"UL -94HB
1/8"UL -94HB
Heat Deflection TemperatureUnannealed18.5kg/cm²,1/2"ASTM D-648103 °C
vicat1.000gASTM D-1525125 °C
mechanical propertiesTest ConditionTest MethodCNOOC&LG HUIZHOU/XR-401
Elongation at breakASTM D-63825 %
flexural modulusASTM D-79022000 kg/cm2
impact elasticityNotched1/4"ASTM D-25616 kgcm/cm
Rockwell hardnessR-ScaleASTM D-785104
tensile strengthASTM D-638460 kg/cm2
Electrical performanceTest ConditionTest MethodCNOOC&LG HUIZHOU/XR-401
arc resistanceASTM D-495PLC_6
Compared to the Leakage Tracking Index (CTI)UL -746A PLCCode
High arc combustion index (HAI)UL -746APLC 0
High Voltage Arc Traceability Rate (HVTR)UL -746APLC 2
Hot wire ignition (HWI)UL -746APLC 5
Physical propertiesTest ConditionTest MethodCNOOC&LG HUIZHOU/XR-401
densityASTM D-7921.05
melt mass-flow rate220℃/10kgASTM D-12386 g/10min
shrinkage rateASTM D-9550.004-0.007 mm/mm