Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | TPI THAILAND/1126NK |
|---|---|---|---|
| elongation | Yield | ASTM D638 | 29 % |
| tensile strength | Yield | ASTM D638 | 35.0 Mpa |
| Bending modulus | 1%Secant | ASTM D790 | 1450 Mpa |
| hardness | Test Condition | Test Method | TPI THAILAND/1126NK |
| Rockwell hardness | R-Scale | ASTM D785 | 105 |
| thermal performance | Test Condition | Test Method | TPI THAILAND/1126NK |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 100 °C |
| impact performance | Test Condition | Test Method | TPI THAILAND/1126NK |
| Charpy Notched Impact Strength | 23°C | DIN 53453 | 3.0 kJ/m² |
| Physical properties | Test Condition | Test Method | TPI THAILAND/1126NK |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 11 g/10min |