Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM EC270TX CELANESE GERMANY
HOSTAFORM®
Fitness equipment,Automotive Applications,Thin walled products
Conductive,High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | CELANESE GERMANY/EC270TX |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 70.0 °C |
Melting temperature | ISO 11357-3 | 166 °C |
mechanical properties | Test Condition | Test Method | CELANESE GERMANY/EC270TX |
---|---|---|---|
Nominal tensile fracture strain | ISO 527-2/1A/50 | 15 % | |
Tensile modulus | ISO 527-2/1A/1 | 1950 Mpa | |
Tensile strain | Yield | ISO 527-2/1A/50 | 11 % |
tensile strength | Yield | ISO 527-2/1A/50 | 44.0 Mpa |
Electrical performance | Test Condition | Test Method | CELANESE GERMANY/EC270TX |
---|---|---|---|
Surface resistivity | IEC 60093 | 1E+03 ohms | |
Volume resistivity | IEC 60093 | 1E+03 ohms·cm |
Physical properties | Test Condition | Test Method | CELANESE GERMANY/EC270TX |
---|---|---|---|
density | ISO 1183 | 1.38 g/cm³ | |
Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 1.50 cm3/10min |
impact performance | Test Condition | Test Method | CELANESE GERMANY/EC270TX |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 6.5 kJ/m² |