Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 VENYL SG209 - 8229 AD MAJORIS FRANCE
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | AD MAJORIS FRANCE/VENYL SG209 - 8229 |
---|---|---|---|
Impact strength of simply supported beam without notch | ISO 179 | 30 kJ/m² | |
Charpy Notched Impact Strength | ISO 179 | 8.0 kJ/m² |
hardness | Test Condition | Test Method | AD MAJORIS FRANCE/VENYL SG209 - 8229 |
---|---|---|---|
Rockwell hardness | L计秤 | ASTM D785 | 102 |
Mechanical properties | Test Condition | Test Method | AD MAJORIS FRANCE/VENYL SG209 - 8229 |
---|---|---|---|
Tensile modulus | ISO 527-2 | 6500 MPa | |
tensile strength | 断裂 | ISO 527-2 | 115 MPa |
Tensile strain | 断裂 | ISO 527-2 | 3.5 % |
Flexural modulus | ISO 178 | 5500 MPa | |
bending strength | ISO 178 | 200 MPa |
Electrical performance | Test Condition | Test Method | AD MAJORIS FRANCE/VENYL SG209 - 8229 |
---|---|---|---|
Surface Resistivity | DIN 53482 | 1E+12 ohms | |
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | PLC 1 |
Volume resistivity | DIN 53482 | 1E+15 ohms·cm |
flammability | Test Condition | Test Method | AD MAJORIS FRANCE/VENYL SG209 - 8229 |
---|---|---|---|
Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 650 °C |
UL flame retardant rating | 1.6mm | UL 94 | HB |
physical property | Test Condition | Test Method | AD MAJORIS FRANCE/VENYL SG209 - 8229 |
---|---|---|---|
Shrinkage rate | 0.40to0.80 % | ||
Water absorption rate | 平衡,23°C,50%RH | 2.6 % | |
density | ISO 1183 | 1.27 g/cm³ |
Thermal performance | Test Condition | Test Method | AD MAJORIS FRANCE/VENYL SG209 - 8229 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 200 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 190 °C | |
melting temperature | ISO 3146 | 220 °C |