PEKK Pyramid™ PEKK KD4219 Polymics, Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
Impact strength of cantilever beam gap | 3.18mm | ASTM D256 | 53 J/m |
Suspended wall beam without notch impact strength | 3.18mm | ASTM D256 | 640 J/m |
Supplementary Information | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
limiting pv value | 142000 J/m |
hardness | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
Shore hardness | 邵氏D | ASTM D2240 | 84 |
Rockwell hardness | M级 | ASTM D785 | 90 |
Mechanical properties | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 2.0 % |
bending strength | 屈服 | ASTM D790 | 248 MPa |
compressive strength | ASTM D695 | 221 MPa | |
tensile strength | 断裂 | ASTM D638 | 172 MPa |
Flexural modulus | ASTM D790 | 12400 MPa | |
Tensile modulus | ASTM D638 | 12400 MPa | |
coefficient of friction | 与钢-动态 | ASTM D1894 | 0.17 |
与钢-静态 | ASTM D1894 | 0.11 | |
shear strength | ASTM D732 | 138 MPa |
Electrical performance | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
Surface Resistivity | ASTM D257 | <1.0E+8 ohms |
flammability | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
UL flame retardant rating | 3.2mm | UL 94 | V-0 |
physical property | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
Water absorption rate | 24hr | ASTM D570 | 0.040 % |
density | ASTM D792 | 1.46 g/cm³ |
Thermal performance | Test Condition | Test Method | Polymics, Ltd./Pyramid™ PEKK KD4219 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 260 °C |
Linear coefficient of thermal expansion | MD:-40到149°C | TMA | 4.5E-05 cm/cm/°C |
Glass Transition Temperature | DSC | 160 °C | |
thermal conductivity | ASTMC177 | 0.25 W/m/K | |
melting temperature | DSC | 360 °C |