Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| Basic Performance | Test Condition | Test Method | TOPAS GERMANY/8007F-500 |
|---|---|---|---|
| density | ISO 1183 | 1.02 g/cm³ | |
| Water absorption rate | Saturation,23℃ | ISO 62 | 0.01 % |
| melt mass-flow rate | 190℃/2.16kg | ISO 1133 | 2 ISO 527-2/5, ISO 527-2/50 |
| mechanical properties | Test Condition | Test Method | TOPAS GERMANY/8007F-500 |
| Elongation at Break | 70um,Cast Film,TD | ISO 527-3 | 3.4 % |
| Tensile modulus | 70um,Cast Film,MD | ISO 527-3 | 2100 MPa |
| 70um,Cast Film,TD | ISO 527-3 | 1700 MPa | |
| tensile strength | 70um,Cast Film,MD | ISO 527-3 | 55 MPa |
| Elongation at Break | 70um,Cast Film,MD | ISO 527-3 | 3.4 % |