Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM Copolymer Ekatal® H 12 Sattler KunststoffWerk GmbH
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Sattler KunststoffWerk GmbH/Ekatal® H 12 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 6.3 kJ/m² |
-30°C | ISO 179/1eA | 4.8 kJ/m² |
Mechanical properties | Test Condition | Test Method | Sattler KunststoffWerk GmbH/Ekatal® H 12 |
---|---|---|---|
Tensile modulus | ISO 527-2 | 3030 MPa | |
tensile strength | 断裂 | ISO 527-2 | 71.4 MPa |
Tensile strain | 断裂 | ISO 527-2 | 16 % |
bending strength | 3.5%应变 | ISO 178 | 81.3 MPa |
Tensile strain | 屈服 | ISO 527-2 | 10 % |
bending strength | -- | ISO 178 | 104 MPa |
tensile strength | 屈服 | ISO 527-2 | 72.5 MPa |
Flexural modulus | ISO 178 | 2870 MPa |
physical property | Test Condition | Test Method | Sattler KunststoffWerk GmbH/Ekatal® H 12 |
---|---|---|---|
density | ISO 1183 | 1.42 g/cm³ | |
melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 12 g/10min |
Thermal performance | Test Condition | Test Method | Sattler KunststoffWerk GmbH/Ekatal® H 12 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/Af | 102 °C |
Linear coefficient of thermal expansion | MD:20到52°C | ISO 11359-2 | 1E-04 cm/cm/°C |
TD:52到117°C | ISO 11359-2 | 1.2E-04 cm/cm/°C | |
TD:20到52°C | ISO 11359-2 | 9.4E-05 cm/cm/°C | |
MD:52到117°C | ISO 11359-2 | 1E-04 cm/cm/°C |