Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPE EM460 DSM HOLAND
Arnite®
Electrical applications、Automotive Applications
High impact resistance、Low temperature resistanc
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | DSM HOLAND/EM460 |
---|---|---|---|
Shore hardness | 邵氏D,3秒 | ISO 868 | 40 |
Electrical performance | Test Condition | Test Method | DSM HOLAND/EM460 |
---|---|---|---|
dielectric strength | IEC 60243-1 | 20 KV/mm | |
Volume resistivity | IEC 60093 | 1E+13 ohms·cm | |
relative permittivity | 1MHz | IEC 60250 | 4.40 |
Dissipation Factor | 1MHz | IEC 60250 | 0.035 |
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | V |
Mechanical properties | Test Condition | Test Method | DSM HOLAND/EM460 |
---|---|---|---|
Tensile modulus | ISO 527-2 | 85.0 Mpa | |
Nominal tensile fracture strain | ISO 527-2 | 800 % | |
tensile strength | 10%应变 | ISO 527-2 | 6.60 Mpa |
断裂 | ISO 527-2 | 23.0 Mpa | |
50%应变 | ISO 527-2 | 9.20 Mpa | |
5.0%应变 | ISO 527-2 | 3.90 Mpa | |
100%应变 | ISO 527-2 | 9.30 Mpa |
flammability | Test Condition | Test Method | DSM HOLAND/EM460 |
---|---|---|---|
Flammability level | 1.6mm | IEC 60695-11-10,-20 | HB |
physical property | Test Condition | Test Method | DSM HOLAND/EM460 |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 1.5 % |
MD | ISO 294-4 | 1.3 % | |
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | 0.30 % |
饱和,23°C | ISO 62 | 0.70 % | |
Melt volume flow rate | 230°C/2.16kg | ISO 1133 | 46.0 cm3/10min |
Thermal performance | Test Condition | Test Method | DSM HOLAND/EM460 |
---|---|---|---|
melting temperature | ISO 11357-3 | 189 °C | |
vicat | ISO 306/B50 | 50.0 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 1.6E-04 cm/cm/°C |
TD | ISO 11359-2 | 1.6E-04 cm/cm/°C |
Contact Us
Get App
Top