Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

SPS 450 DUPONT-DOW US
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
film | Test Condition | Test Method | DUPONT-DOW US/450 |
---|---|---|---|
film thickness | 1.0 mil | ||
tensile strength | MD : 断裂, 51 µm | ASTM D882 | 26.2 Mpa |
Usage - Calculated | 25.4µm | 内部方法 | 39.3 m²/kg |
elongation | TD:断裂,25µm | ASTM D882 | 550 % |
Water Vapor Transmission Rate | 38℃, 51 µm, 90% RH | ASTM F1249 | 0.14 g/m²/24 hr |
Heat sealing strength | MD : 177℃ | 内部方法 | 890 N/m |
usage | 50.8 µm | ASTM D4321 | 39.3 m²/kg |
tensile strength | TD:断裂,25µm | ASTM D882 | 18.6 Mpa |
elongation | MD:断裂,25µm | ASTM D882 | 400 % |
MD : 断裂, 51 µm | ASTM D882 | 400 % | |
film thickness | 1.0mil(25µ | ||
经测试 | ASTM D374 | 25 µm | |
tensile strength | MD:断裂,25µm | ASTM D882 | 26.2 Mpa |
OTr | 23°C,25µm,50%RH | ASTM D3985 | 0.33 cm³·mm/m²/atm/24hr |
Heat sealing strength | 177°C,25.4µm | 内部方法 | 890 g/2.5cm |
film thickness | 25 µm | ||
Water Vapor Transmission Rate | 25µm,38°C,90%RH | ASTMF1249 | 0.14 g·mm/m²/atm/24hr |
OTr | 23℃, 51 µm, 50% RH | ASTM D3985 | 0.33 g/m²/24 hr |
Mechanical properties | Test Condition | Test Method | DUPONT-DOW US/450 |
---|---|---|---|
coefficient of friction | 与自身-动态 | ASTM D1894 | 0.20 |
Contact Us
Get App
Top