| Physical properties | Test Condition | Test Method | DUPONT USA/6130 BK |
|---|---|---|---|
| Water absorption rate | ASTM D570/ISO 62 | 0.002 % | |
| density | ASTM D792/ISO 1183 | 1.62 | |
| thermal performance | Test Condition | Test Method | DUPONT USA/6130 BK |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 277 ℃(℉) |
| Combustibility (rate) | UL 94 | V-0(0.2) | |
| Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 1.3(3.7) mm/mm.℃ | |
| mechanical properties | Test Condition | Test Method | DUPONT USA/6130 BK |
| tensile strength | ASTM D638/ISO 527 | 150 kg/cm²(MPa)[Lb/in²] | |
| Impact strength of cantilever beam gap | ASTM D256/ISO 179 | 108 kg·cm/cm(J/M)ft·lb/in | |
| bending strength | ASTM D790/ISO 178 | 170 kg/cm²(MPa)[Lb/in²] | |
| elongation | ASTM D638/ISO 527 | 2.7 % |