Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PBT 3316 JAPAN POLYPLASTIC
DURANEX®
Fitness equipment,Casters
Glass fiber reinforced
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | JAPAN POLYPLASTIC/3316 |
---|---|---|---|
Surface Resistivity | --- | --- | 1×1016 Ω |
arc resistance | *2 | --- | 92 S |
*2 | --- | 250 V |
Basic performance | Test Condition | Test Method | JAPAN POLYPLASTIC/3316 |
---|---|---|---|
density | --- | ASTM D-792 | 1.66 --- |
Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/3316 |
---|---|---|---|
Surface Resistivity | ASTM D257/IEC 60093 | 1×10^16 Ω | |
Volume resistivity | 3mmt | ASTM D-257 | 1×1016 Ω.cm |
ASTM D257/IEC 60093 | 1×10^16 Ω.cm | ||
dielectric strength | 短时:3mmt | ASTM D-149 | 20 MV/m |
Mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/3316 |
---|---|---|---|
bending strength | ASTM D790/ISO 178 | 225 kg/cm²(MPa)[Lb/in²] | |
tensile strength | --- | ASTM D-638 | 147 Mpa |
Flexural modulus | ASTM D790/ISO 178 | 9610 kg/cm²(MPa)[Lb/in²] | |
Impact strength of cantilever beam gap | 缺口,--- | ASTM D-256 | 98 J/m |
Charpy Notched Impact Strength | ASTM D256/ISO 179 | 98 kg·cm/cm(J/M)ft·lb/in | |
elongation at break | ASTM D638/ISO 527 | 2.7 % | |
Flexural modulus | --- | ASTM D-790 | 9610 Mpa |
Impact strength of cantilever beam gap | 反缺口侧,--- | ASTM D-256 | 680 J/m |
tensile strength | ASTM D638/ISO 527 | 147 kg/cm²(MPa)[Lb/in²] | |
bending strength | --- | ASTM D-790 | 225 Mpa |
elongation at break | --- | ASTM D-638 | 2.7 % |
other | Test Condition | Test Method | JAPAN POLYPLASTIC/3316 |
---|---|---|---|
characteristic | GF30% |
Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/3316 |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.66 |
Thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/3316 |
---|---|---|---|
Combustibility (rate) | UL 94 | V-0 | |
UL flame retardant rating | --- | UL 94 | V-0 --- |
Linear coefficient of thermal expansion | 室温 | --- | 2-7 ×10-5/℃ |
Heat distortion temperature | 1.82MPa,HDT | ASTM D-648 | 212 °C |
HDT | ASTM D648/ISO 75 | 212 ℃(℉) | |
Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 2-7 mm/mm.℃ |