Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU 58137 NOVEON USA
ESTANE®
corrugated pipe、Automotive sector、Consumer goods sector、Lawn garden equipment、Industrial applications
High crystallinity、High elasticity、Dimensional stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | NOVEON USA/58137 |
---|---|---|---|
Shore hardness | 邵氏D,5秒 | ASTM D2240 | 62to68 |
Mechanical properties | Test Condition | Test Method | NOVEON USA/58137 |
---|---|---|---|
Taber abraser | 1000Cycles,1000g,CS-17转轮 | ASTM D3389 | 41.0 mg |
Flexural modulus | 23°C | ASTM D790 | 370 Mpa |
elastomer | Test Condition | Test Method | NOVEON USA/58137 |
---|---|---|---|
tear strength | 开裂 | ASTM D470 | 51 kN/m |
tensile strength | 300%应变,0.762mm | ASTM D412 | 31.0 Mpa |
elongation | 断裂,0.762mm | ASTM D412 | 430 % |
compression set | 70°C,22hr | ASTM D395 | 61 % |
tear strength | 0.762mm4 | ASTM D624 | 206 kN/m |
tensile strength | 断裂,0.762mm | ASTM D412 | 41.0 Mpa |
100%应变,0.762mm | ASTM D412 | 21.0 Mpa | |
compression set | 23°C,22hr | ASTM D395 | 42 % |
physical property | Test Condition | Test Method | NOVEON USA/58137 |
---|---|---|---|
Shrinkage rate | MD:--3 | ASTM D955 | 0.80 % |
MD:--2 | ASTM D955 | 0.90 % |
Thermal performance | Test Condition | Test Method | NOVEON USA/58137 |
---|---|---|---|
Glass Transition Temperature | DSC | -15.0 °C | |
melting temperature | DSC | 227 °C |