ABS Niblend S45 Soredi S.p.a.
--
Thin walled components
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Soredi S.p.a./Niblend S45 |
|---|---|---|---|
| Rockwell hardness | ASTM D785 | 115 R |
| thermal performance | Test Condition | Test Method | Soredi S.p.a./Niblend S45 |
|---|---|---|---|
| Hot deformation temperature | 1.80MPaUnannealed | ASTM D648 | 106 °C |
| Vicat softening temperature | ASTM1525 | 115 °C |
| mechanical properties | Test Condition | Test Method | Soredi S.p.a./Niblend S45 |
|---|---|---|---|
| Bending modulus | 23°C | ASTM D790 | 2300 MPa |
| bending strength | 23°C | ASTM D790 | 65 MPa |
| Elongation at Break | 23°C | ASTM D638 | 30 % |
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 400 J/m |
| tensile strength | 23°C | ASTM D638 | 40 MPa |
| flame retardant performance | Test Condition | Test Method | Soredi S.p.a./Niblend S45 |
|---|---|---|---|
| Relative temperature of heating wire | 2.00mm | IEC 60695-2-13 | 650 °C |
| UL flame retardant rating | UL -94 | HB 3.20mm | |
| UL -94 | HB 1.60mm |
| Physical properties | Test Condition | Test Method | Soredi S.p.a./Niblend S45 |
|---|---|---|---|
| density | ASTM D792 | 1.10 g/cm³ | |
| melt mass-flow rate | 260℃/5.0Kg | ASTM D1238 | 20 g/10min |
| Shrinkage rate | MD | ASTM D995 | 0.50-0.80 % |