Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Polyester PM471 DSM Additive Manufacturing
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | DSM Additive Manufacturing/ PM471 |
|---|---|---|---|
| Shore hardness | ShoreD,3Sec | ISO 868 | 44 |
| thermal performance | Test Condition | Test Method | DSM Additive Manufacturing/ PM471 |
|---|---|---|---|
| Melting temperature | ISO 11357-3 | 217 °C |
| mechanical properties | Test Condition | Test Method | DSM Additive Manufacturing/ PM471 |
|---|---|---|---|
| Nominal tensile fracture strain | ISO 527-2 | 220 % | |
| Tensile modulus | ISO 527-2 | 150 MPa | |
| tensile strength | Break | ISO 527-2 | 16.5 MPa |
| 50%Strain | ISO 527-2 | 12.2 MPa | |
| 5.0%Strain | ISO 527-2 | 6.20 MPa | |
| 100%Strain | ISO 527-2 | 13.9 MPa | |
| 10%Strain | ISO 527-2 | 8.70 MPa |
| Physical properties | Test Condition | Test Method | DSM Additive Manufacturing/ PM471 |
|---|---|---|---|
| density | ISO 1183 | 1.20 g/cm³ | |
| Melt Volume Flow Rate (MVR) | 230°C/2.16kg | ISO 1133 | 12.5 cm³/10min |
| impact performance | Test Condition | Test Method | DSM Additive Manufacturing/ PM471 |
|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 无断裂 |
| 23°C | ISO 179/1eA | 无断裂 | |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 无断裂 |
| -30°C | ISO 180/1A | 无断裂 |