Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

MVLDPE 2038.68G STYRON US
DOWLEX™
--
Processing aids
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | STYRON US/2038.68G |
---|---|---|---|
Elmendorf tear strength | ASTM D1922 | 16.3 g/micron | |
Film toughness | 25.4um,TD | ASTM D-882 | 115 J/cm4 |
25.4um,MD | ASTM D-882 | 97.5 J/cm³ | |
impact force | ASTM D882 | 1389 ft-lbf/in3 | |
Thin film puncture strength | 25.4um | Internal Method | 7.69 J/cm³ |
Basic Performance | Test Condition | Test Method | STYRON US/2038.68G |
---|---|---|---|
density | ASTM D-792 | 0.935 g/m3 | |
melt mass-flow rate | 190℃/2.16kg | ASTM D-1238 | 1 g/10min |
machinability | Test Condition | Test Method | STYRON US/2038.68G |
---|---|---|---|
Melt Temperature | 204-246 °C |
thermal performance | Test Condition | Test Method | STYRON US/2038.68G |
---|---|---|---|
Melting temperature | Internal Method | 126 °C | |
Vicat softening temperature | ASTM D-1525 | 120 °C | |
ASTM1525 | 120 °C | ||
Melting Temperature | 陶氏化学方法(DSC | 126 °C |
mechanical properties | Test Condition | Test Method | STYRON US/2038.68G |
---|---|---|---|
Dart impact | 25.4um | ASTM D-1709A | 110 g |
ASTM D1709 | 112 g | ||
Elmendorf tear strength | 25.4um,MD | ASTM D-1922 | 71 g |
25.4um,TD | ASTM D-1922 | 410 g | |
ASTM D192 | 71 g | ||
elongation | Break | ASTM D882 | 656 % |
Elongation at Break | 25.4um,TD | ASTM D-882 | 660 % |
25.4um,MD | ASTM D-882 | 520 % | |
impact force | 93 ft-lbf/in3 | ||
Secant modulus | ASTM D882 | 348.5 Mpa | |
tensile strength | 25.4um,Yield,TD | ASTM D-882 | 16.7 Mpa |
25.4um,TD,Break | ASTM D-882 | 33.1 Mpa | |
25.4um,MD,Break | ASTM D-882 | 38.3 Mpa | |
ASTM D882 | 33.13 Mpa | ||
25.4um,Yield,MD | ASTM D-882 | 15.2 Mpa |
Physical properties | Test Condition | Test Method | STYRON US/2038.68G |
---|---|---|---|
melt mass-flow rate | ℃/Kg | ASTM D1238 | 1.0 g/10min |
厚度 | 25.4 microns |
optical performance | Test Condition | Test Method | STYRON US/2038.68G |
---|---|---|---|
gloss | 45°,25.4um | ASTM D-2457 | 58 |
ASTM2457 | 58 | ||
turbidity | 25.4um | ASTM D-1003 | 7 % |
ASTM D1003 | 7.0 % |