| thermal performance | Test Condition | Test Method | DUPONT USA/HTN51G451HSL |
|---|---|---|---|
| RTI Elec | °C | 140to150 | |
| 1.8MPa, annealed | °C | 283to300 | |
| RTI Imp | °C | 118to150 | |
| 1.8MPa, unannealed | °C | 247to292 | |
| Vicat softening temperature | °C | 258to313 | |
| 8.0Mpa, unannealed | °C | 165to230 | |
| 0.45MPa, annealed | °C | 296to320 | |
| flow | mm/mm/°C | 195.6E-5-25.4E-5 | |
| transverse | mm/mm/°C | 68.6E-5-127.0E-5 | |
| 0.45MPa, unannealed | °C | 275to308 | |
| Continuous use temperature | °C | 140to186 | |
| RTI | °C | 119to150 | |
| flammability | Test Condition | Test Method | DUPONT USA/HTN51G451HSL |
| Extreme Oxygen Index | % | 23to25 | |
| Burning wire flammability index | °C | 743to960 | |
| Hot filament ignition temperature | °C | 721to926 | |
| mechanical properties | Test Condition | Test Method | DUPONT USA/HTN51G451HSL |
| Fracture, 23 ℃ | 108.28to262.76 MPa | ||
| % | 1.5to3.1 | ||
| shear strength | 23℃ | 88.28to107.59 MPa | |
| Yield, 23 ℃ | 12.62to270.34 MPa | ||
| compressive strength | 23℃ | 142.76to196.55 MPa | |
| Yield, 23 ℃ | % | 1.5to2.6 | |
| Poisson's ratio | 23℃ | 0.41 | |
| Tensile modulus | 摩擦系数 | 0.15to0.52 | |
| hardness | Test Condition | Test Method | DUPONT USA/HTN51G451HSL |
| Rockwell hardness | 23℃ | 125 | |
| Physical properties | Test Condition | Test Method | DUPONT USA/HTN51G451HSL |
| Lateral flow: 23 ℃ | Across Flow, 23℃ | mm/mm | 119.4E-3-0.254 |
| 23℃,24hr | % | 0.30to0.51 | |
| Balance, 23 ℃, 50% RH | % | 0.21to1.2 | |
| Flow: 23 ℃ | Flow,23℃ | mm/mm | 48.3E-3-129.5E-3 |
| impact performance | Test Condition | Test Method | DUPONT USA/HTN51G451HSL |
| Impact strength of simply supported beam without notch | 23℃ | kJ/m² | 4.178to19.964 |