Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| thermal performance | Test Condition | Test Method | SICHUAN DEYANG/PPS-hMR61 |
|---|---|---|---|
| UL flame retardant rating | V-0 | ||
| Hot deformation temperature | HDT | 267 °C | |
| Melting temperature | 289 °C | ||
| Physical properties | Test Condition | Test Method | SICHUAN DEYANG/PPS-hMR61 |
| Shrinkage rate | 平行 | 0.25 % | |
| 垂直 | 0.75 % | ||
| Electrical performance | Test Condition | Test Method | SICHUAN DEYANG/PPS-hMR61 |
| Dielectric loss | 1MHz | 0.010 | |
| Surface resistivity | 2×1015 Ω | ||
| Dielectric strength | 15 KV/mm | ||
| Volume resistivity | 4×1014 Ω.m | ||
| Dielectric constant | 1MHz | 5.0 | |
| mechanical properties | Test Condition | Test Method | SICHUAN DEYANG/PPS-hMR61 |
| Bending modulus | 1.63×104 Mpa | ||
| compressive strength | 130 Mpa | ||
| bending strength | 234 Mpa | ||
| Rockwell hardness | 95 hr | ||
| tensile strength | 159 Mpa | ||
| Impact strength of cantilever beam gap | 12 kJ/m² | ||
| elongation | Break | 2.5 % | |
| Basic Performance | Test Condition | Test Method | SICHUAN DEYANG/PPS-hMR61 |
| density | 1.92 g/cm³ |