Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP HP741T LYONDELLBASELL HOLAND
Moplen
Thin walled packaging、container、Thin walled packaging con
Food contact level、It is an additional high
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP741T |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 80 |
Basic performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP741T |
---|---|---|---|
density | Method D | ISO 1183 | 0.9 g/cm³ |
melt mass-flow rate | 230°C/2.16 kg | ISO 1133 | 60 g/10min |
Mechanical properties | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP741T |
---|---|---|---|
Shore hardness | Shore D | ISO 868 | 80 |
Flexural modulus | ISO 178 | 1700 Mpa | |
tensile strength | Yield | ISO 527-1 | 36 Mpa |
屈服 | ISO 527-2 | 36.0 Mpa | |
Impact strength of cantilever beam gap | 23℃ | ISO 180/1A | 1.8 |
physical property | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP741T |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 60 g/10min |
Thermal performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/HP741T |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 98.0 °C |
vicat | A (10N) | ISO 306 | 150 °C |
Heat distortion temperature | 0.45Mpa, Unannealed,HDT | ISO 75B-1 | 98 °C |
vicat | ISO 306/A | 150 °C |
Contact Us