HIPS SEHI-117 IDEMITSU MALASIA
--
Shell
Characteristics, high fluidity, flame retardancy, form, particles
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | IDEMITSU MALASIA/SEHI-117 |
|---|---|---|---|
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 76.0 °C |
| mechanical properties | Test Condition | Test Method | IDEMITSU MALASIA/SEHI-117 |
|---|---|---|---|
| elongation | Break | ASTM D638 | 45 % |
| tensile strength | Break | ASTM D638 | 23.5 MPa |
| Physical properties | Test Condition | Test Method | IDEMITSU MALASIA/SEHI-117 |
|---|---|---|---|
| density | ASTM D792 | 1.15 g/cm³ | |
| melt mass-flow rate | 200°C/5.0 kg | ASTM D1238 | 15 g/10 min |
| flammability | Test Condition | Test Method | IDEMITSU MALASIA/SEHI-117 |
|---|---|---|---|
| UL flame retardant rating | 3.00 mm | UL 94 | V-0 |
| squeeze out | Test Condition | Test Method | IDEMITSU MALASIA/SEHI-117 |
|---|---|---|---|
| drying temperature | 70.0 °C | ||
| drying time | 1.0 to 2.0 hr | ||
| Material barrel temperature | 200 to 240 °C | ||
| Oral mold temperature | 190 to 220 °C |
| injection | Test Condition | Test Method | IDEMITSU MALASIA/SEHI-117 |
|---|---|---|---|
| drying temperature | 70.0 °C | ||
| drying time | 1.0 to 2.0 hr | ||
| Mold temperature | 40.0 to 60.0 °C | ||
| Spray nozzle temperature | 200 to 230 °C | ||
| Temperature at the front of the material cylinder | 210 to 240 °C | ||
| Temperature at the rear of the barrel | 180 to 210 °C | ||
| Temperature in the middle of the barrel | 190 to 220 °C |