EVA 18-0.7 BEIJING EASTERN
--
Medical membrane
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | BEIJING EASTERN/18-0.7 |
|---|---|---|---|
| density | ASTM D-1505 | 0.940 | |
| melt mass-flow rate | ASTM D-1238 | 0.7 g/10 |
| thermal performance | Test Condition | Test Method | BEIJING EASTERN/18-0.7 |
|---|---|---|---|
| Melting temperature | 87 °C | ||
| Vicat softening temperature | ASTM D-1525 | 70 °C |
| mechanical properties | Test Condition | Test Method | BEIJING EASTERN/18-0.7 |
|---|---|---|---|
| Elongation at Break | ASTM D-6398 | 640 % | |
| Impact strength of cantilever beam gap | ASTM D-1709 A-B | 大于等于300 g | |
| Shore hardness | ASTM D-2240 | 89 | |
| tear strength | ASTM D-1922 | 151 g | |
| tensile strength | Break | ASTM D-638 | 33 N/mm |
| Yield | ASTM D-638 | 4.5 N/mm |
| Electrical performance | Test Condition | Test Method | BEIJING EASTERN/18-0.7 |
|---|---|---|---|
| Dielectric constant | ASTM D-150 | 3.1 | |
| Dielectric strength | ASTM D-149 | 650 KV/cm |
| Physical properties | Test Condition | Test Method | BEIJING EASTERN/18-0.7 |
|---|---|---|---|
| film thickness | 40 u | ||
| gloss | ASTM D-1003A | 85 % | |
| turbidity | ASTM D-2457 | 1.4 % | |
| Vinyl acetate content | ISC.DIS 8965/1989(E) | 18 % |